Fibre Composite Product
Basalt fiber is used mainly
Continuous Basalt Fiber
Using natural volcanic basalt as raw material, after melting at 1450 ~ 1500 ℃, the fiber is made by high - speed drawing of platinum alloy.
Basalt fiber is an excellent alternative to other materials:
Light weight, density is 1 / 3 of steel; High strength, superior to steel and most other composite materials; High temperature resistance, good thermal stability; High stability and good compatibility with other materials; Good dielectric properties, can prevent radiation; The penetrate performance and the wave absorbing property are excellent. Acid and alkali corrosion.
Basalt fiber composite material
Like mobile phones, the internet, GPS and other technologies, basalt fiber was born in the former Soviet union in the 1960s, used in the military field. Now in our country, basalt fiber composite material is widely used in military, aerospace field, used as rocket spoiler, missile launcher and so on. The products in the civil field need to be developed urgently.
Because the basalt fiber composite material has the characteristics of high strength and high module, it also has high temperature and low temperature performance ( - 269 - 650 ℃ ), anti - alkali, anti - oxidation, anti - radiation, adiabatic sound insulation, fire retardant, good filtering, high compression strength and shear strength, it can adapt to the use of various environments and so on. The oil and chemical fiber composite prepared by basalt fiber composite materials in the pipeline adapts to the complex working conditions environment in the petrochemical, coal chemical, general chemical industry and so on, meets the special requirements of high temperature, high pressure, low temperature resistance, corrosion resistance, wear resistance and low temperature performance, and is light and easy to install. In the petroleum and natural gas chemical industry, coal chemical industry, general chemical industry and other fields of application has broad development space and great development value.
-------------------------------------------------------------------------------------------------------------------------------------------------- |
On-site comparison |
Traditional PipeThe pipeline perforation due to stress corrosion and galvanic corrosion occurred after 6 months of use of the cooler duplex stainless steel pipeline in a refinery. |
Composite PipeIn a petrochemical plant, no perforation was found after 6 months of trial operation. no corrosion, no corrosion and no materials were found. after the test, the samples were cut off to check for no corrosion, no media and impurities were attached to the wall, which showed excellent corrosion resistance. |
---|
-------------------------------------------------------------------------------------------------------------------------------------------------- |